Ningbo haijiang machinery manufacturing co.,Ltd

Haijia Injection Machine,Energy Saving More

Manufacturer from China
Verified Supplier
8 Years
Home / Products / Energy Saving Injection Molding Machine /

High Performance Plastic Mold Making Machine HJF80 Ton For Plasic Products

Contact Now
Ningbo haijiang machinery manufacturing co.,Ltd
Visit Website
City:ningbo
Province/State:zhejiang
Contact Person:MrMichael
Contact Now

High Performance Plastic Mold Making Machine HJF80 Ton For Plasic Products

Ask Latest Price
Video Channel
Brand Name :HAIJIA
Model Number :HJF80
Certification :CE ISO9001
Place of Origin :CHINA
MOQ :1 set
Price :Negotiation
Payment Terms :L/C, D/A, D/P, T/T, Western Union, MoneyGram
Supply Ability :100 Set/Sets per Month
Delivery Time :20-30days
Packaging Details :Standard Export Package for Injection Machine
Voltage :Customed Avaiable
Used for :Plasic Products
Motor :servo & standard & variable pump
Keyword :energy saving
Warranty :18 months
Plastic type :Thermoplastic
more
Contact Now

Add to Cart

Find Similar Videos
View Product Description

The shrinkage problem of hard rubber parts (surface concave shrinkage and internal shrinkage) is caused by the defect that the space left by the concentrated shrinkage can not be adequately supplemented by the melt from the direction of the inlet when the melt is cooled and contracted. Therefore, factors that are not conducive to the subsidy will affect us to solve the problem of shrinkage.

Most people know that die temperature is too high to cause shrinkage problems, usually like to reduce the temperature of the die to solve the problem. But sometimes if the die temperature is too low, it is not conducive to solve the shrinkage problem, which is not noticed by many people.

Mold temperature is too low, melt glue cooling is too fast, slightly thicker glue level is far from the water inlet. Because the middle part is cooled too fast, the shrinkage channel is blocked and the melt glue can not be adequately supplemented in the distance, which makes the shrinkage problem more difficult to solve. The shrinkage problem of thick injection parts is particularly prominent.

Moreover, too low die temperature is not conducive to increase the overall shrinkage of injection parts, so that the concentrated shrinkage increases, shrinkage problem is more serious.

Therefore, when solving the difficult shrinkage problem, it is good to remember to check the die temperature. Experienced technicians usually touch the surface of the die cavity with their hands. Each material has its appropriate die temperature. For example, the shrinkage of PC material will be improved if the hole is properly pressed, but if the die temperature is too high, the shrinkage of injection parts will occur.